Product description

A431-2 table adjustment: There will be many holes in the processing process of aluminum alloy workpieces, especially the small holes in the product or the edge gaps of injection molded parts, after anodizing, although these holes, small holes and gaps have been washed, there is still a lot of electrolyte residue, and the electrolyte will gush out during coloring, causing the undesirable phenomenon that the local cannot be colored. This product is suitable for the treatment process of aluminum alloy anode before coloring, which can effectively reduce the occurrence of poor coloring. Product features: 1. Effectively prevent poor coloring caused by insufficient washing; 2. Effectively prevent poor coloring caused by sulfuric acid electrolyte gushing out of holes and screw holes; 3. Yes

Product Features:

1. Effectively prevent poor coloring caused by insufficient washing;
2. Effectively prevent poor coloring caused by sulfuric acid electrolyte gushing out of holes and screw holes;

3. It can extend the life of the coloring solution;